Welina mai i kā mākou mau pūnaewele!

2507 kila kila 5*1 mm paipu wili

ʻO ka wehewehe pōkole:

S32750 2507 F53 1.4410 Huina kemika o ke kila kila

C≤ Si≤ Mn≤ P≤ S≤ Cr≥ Ni≥ Mo≥ N≤
0.03 0.80 2.00 0.030 0.020 24.0-26.0 6.0-8.0 3.0-5.0 0.24-0.32

S32750 (2507, F53, 1.4410) super duplex stainless steel waiwai kino a me mechanical:

1. S32750 (2507, F53, 1.4410) mānoanoa kila lua: 8.0g/cm3.
2. Ka ikaika tensile o S32750 (2507, F53, 1.4410) duplex kila ikaika o ka hoʻonui: σb≥800Mpa.
S32750 (2507, F53, 1.4410) ʻelua ʻāpana kila e hoʻoulu ai i ka ikaika: σ0.2≥550Mpa
4, S32750 (2507, F53, 1.4410) duplex kila elongation: δ≥15%.
5. S32750 (2507, F53, 1.4410) ʻelua ʻāpana kila paʻakikī (HB): 310


Huahana Huahana

Huahana Huahana

2507 Paipu Paipu Kuhili ʻole,S32750 Paipu Kūleʻa Kūleʻa,F53 Paipu Kuhili ʻole,1.4410Paipu Paipu Kuhiliʻole

wehewehe:

S32750 (2507, F53, 1.4410) super duplex stainless steel he 25% chromium, 4% molybdenum a me 7% nickel.
ʻO S32750 ka lua-phase kila he ikaika ikaika a me ka pale ʻana i ka corrosion, ka mea i hoʻohana nui ʻia i ka hana kemika, ʻoihana petrochemical a me nā lako submarine.
ʻO S32750 ʻelua ʻāpana kila ke kūpaʻa ikaika i ka chloride corrosion, kiʻekiʻe thermal conductivity a me ka haʻahaʻa haʻahaʻa hoʻonui hoʻonui.
ʻO ka maʻiʻo kiʻekiʻe o ka chromium, molybdenum a me ka nitrogen he kiʻekiʻe ke kū'ē i ka ʻike ʻana i ka corrosion, crack corrosion a me ka corrosion maʻamau.
Loaʻa i ka S32750 ke kila lua-phase ka ikaika hopena kiʻekiʻe a ʻaʻole kūpono no ka hoʻohana ʻana i nā mahana ma luna o 570 ° c, kahi e emi ai kona paʻakikī i ka manawa.
ʻO S32750 ʻelua ʻāpana kila i hoʻohui i nā kila ferritic a me ke kila austenitic ka waiwai maikaʻi loa, no ka mea, ʻoi aku ka kiʻekiʻe o ka chromium a me ka molybdenum maʻiʻo, no laila ke kūpaʻa maikaʻi loa i ka corrosion, crevice corrosion a me ka hiki o ka corrosion like, duplex microstructure e hōʻoia i ka kila i ka hiki o ke kiʻekiʻe kū'ē i stress corrosion māwae, a me ka mechanical ikaika kiʻekiʻe.

S32750 2507 F53 1.4410 Huina kemika o ke kila kila

C≤ Si≤ Mn≤ P≤ S≤ Cr≥ Ni≥ Mo≥ N≤
0.03 0.80 2.00 0.030 0.020 24.0-26.0 6.0-8.0 3.0-5.0 0.24-0.32

S32750 (2507, F53, 1.4410) super duplex stainless steel waiwai kino a me mechanical:

1. S32750 (2507, F53, 1.4410) mānoanoa kila lua: 8.0g/cm3.
2. Ka ikaika tensile o S32750 (2507, F53, 1.4410) duplex kila ikaika o ka hoʻonui: σb≥800Mpa.
S32750 (2507, F53, 1.4410) ʻelua ʻāpana kila e hoʻoulu ai i ka ikaika: σ0.2≥550Mpa
4, S32750 (2507, F53, 1.4410) duplex kila elongation: δ≥15%.
5. S32750 (2507, F53, 1.4410) ʻelua ʻāpana kila paʻakikī (HB): 310

S32750 (2507, F53, 1.4410) ʻoi loa ke kūʻai ʻana i ke kila kila kila nui loa:

2507 kila kila 5*1 mmpaipu wiliwili

1. Ke hoʻohālikelike ʻia me 904L, S32750 ʻelua-phase kila i ʻoi aku ka ikaika o ka corrosion kū'ē i ka dilute sulfuric acid i hui pū ʻia me nā ion chloride.
ʻO 904L kahi huila austenitic i hoʻolālā kūikawā ʻia e pale aku i ka ʻino o ka sulfuric acid maʻemaʻe.
ʻO ke kiʻekiʻe o ka chromium a me ka molybdenum maʻiʻo o S32750 pālua-phase kila e ʻoi aku ka paʻa ʻana i ka corrosion holoʻokoʻa o nā waikawa organik e like me ka waikawa a me ka acetic acid.
ʻO S32750 duplex steel hoʻi he kūpaʻa kūpaʻa ikaika i nā ʻakika inorganic, ʻoi aku ka nui o nā chlorides.
ʻAʻole hiki ke hoʻohana ʻia ka papa 316L i nā kaiapuni hydrochloric acid kahi i hiki ke hoʻopili ʻia i ka ʻino kūloko a honua paha.
Hiki ke hoʻohana ʻia ke kila kila lua S32750 i loko o ka dilute hydrochloric acid environment, me ke kūpaʻa ikaika i ka ʻike ʻana i ka pōʻino a me ka hiki ʻana o ka corrosion.
2. Intercrystalline corrosion S32750 lua-phase kila he haʻahaʻa kalapona maʻiʻo, e hoemi loa i ka pilikia o ka intercrystalline carbide ua i ka wā wela.No laila, kūpaʻa loa kēia huila i ka corrosion intercrystalline pili carbon.
3. Stress corrosion pohā: ma muli o kona kiʻekiʻe o ka mea hao, ʻoi aku ka maikaʻi o ka pale ʻana a me ka ikaika o S32750 lua-phase kila ma mua o ka 2205.
ʻO S32750 pālua - ʻoi aku ka ʻoi aku o ka pale ʻana i ke koʻikoʻi i ka hiki ʻana i ka pohā ʻino.
4, corrosion a corrosion: nui nā ala e hoʻāʻo ai i ka pale ʻana o nā huahana kila i ka hopena i loaʻa ka chloride.Hōʻike ʻia ka mahana koʻikoʻi no ka ʻino a me ka ʻino o ke kila kila kila ma 1M sodium chloride solution.
Hōʻike nā hopena hoʻokolohua like ʻole i ka S32750 pālua - ʻoi aku ka maikaʻi o ka pale ʻana i ka corrosion.
5, māwae pōʻalo: nā māwae i loko o ka hale a me nā mea ʻē aʻe he aneane hiki ʻole ke pale aku i ke kila kuhiliʻole i ka corrosion i loko o ka chloride environment.2507 pālua - ʻāpana kila i ka ikaika anti - māwae corrosion hiki.

S32750 (2507, F53, 1.4410) kila kila ʻoi loa

2507 kila kila 5*1 mm paipu wili
1. ʻO nā meaʻoihanaʻaila a me ke kinoea
2. ʻO ka paepae waho, ka mea hoʻololi wela, nā mea hana ma lalo o ka wai, nā mea hana ahi
3. ʻOihana hana kemika, ʻoihana moku a me ka paipu,
4. Nā mea kanu desalination, nā mea kanu RO kiʻekiʻe a me nā paipu submarine;
5. Nā ʻāpana mīkini (ikaika kiʻekiʻe, ʻāpana anti-corrosion)
6, ʻoihana ikehu ʻōnaehana FGD, ʻōnaehana holoi ʻoihana, hale kiaʻi absorption.

S32750 (2507, F53, 1.4410) super duplex stainless steel kiko'ī a me ke kūlana lako:
1, hoʻokaʻawale ʻokoʻa: S32750 paipu ʻole, S32750 pā kila, S32750 pōʻai kila, S32750 forging, S32750 flange, S32750 apo,S32750 paipu wiliwili, S32750 kāʻei kila, S32750 mea uea a me S32750 kākoʻo mea kuʻihao.
2, kūlana hāʻawi: ʻaʻa ʻole ʻia: ka hopena paʻa + keʻokeʻo waikawa, hiki ke hoʻopaʻa ʻia ka lōʻihi;
Papa: hoʻonā paʻa, pickling, ʻoki ʻoki;
Paipu welded: solution acid ke'oke'o
Bar ma ke kālai ʻana i ke kūlana ʻōwili, hoʻoliʻiliʻi ʻili a i ʻole ka polishing;
Ma hope o ka'ōwili anu, ka ho'ohehe'e pa'a i ke kūlana palupalu, ka hā'awi 'ana i ka ili;
Hāʻawi ʻia ka mea silika ma ke ʻano o ka poli maikaʻi ma ke ʻano o ka pahu pickling solution paʻa a i ʻole ke kaula pololei.

 


https://www.shcoiledtube.com/

https://www.shcoiledtube.com/

https://www.shcoiledtube.com/

https://www.shcoiledtube.com/


  • Mua:
  • Aʻe:

  • E kākau i kāu leka ma aneʻi a hoʻouna mai iā mākou